Default Re: Polishing or Chroming Aluminum?

all you gurus out there can correct me if i'm wrong but, chroming the frame and swing arm is craziness. You would need to polish first anyway. The small parts should be easy. I'm sure CASWELL would answer your plating questions more quickly in the metal plating forum, or you may find the answer you are looking for there. As far as polishing goes, it is a fine art. It doesnt take forever but you really need to take your time. The more you rush the worse it turns out. Check out the replies on some of the other topics. It will outline the steps to polishing clearly. These guys are really helpful. My TL1000R is near finished and a GSXR750 racebike is already out the door. I could not have done it with out this forum.