Anodizing Multiple Pieces
I'm fairly new at this and had question about anodizing multiple pieces. How important is it that every thing in the run is close to the same size(surface area)?
I made a run today with three pieces that were 16, 46 and 69 sq in. (131 total). I ran at 6 a/sf (5.5 amps) for 108 minutes shooting for 0.9 thickness. It appears that the smallest piece turned out the best (It seemed to take the black dye better).
Thanks for your help.
Dean
|