Default Re: Titanium Motorcycle Exhaust Question ?

You can buff it like SS with a sisal buff, just use the compound more often and expect it to take a bit longer. You can forget about sanding it, I found that buffing it seems to move more metal than most sandpaper. It can be brought to a very high luster, it just seems to take forever. The bluing will keep coming back, there is nothing you can do about that.
If you buff it you will have to buff all the visible areas because it will alter the look of the original finish.