Default Re: Another Blasting media question

Thanks....think I'll go with a finer grade & put up with the dust in the cabinet.Matter of fact I just took my cabinet all apart & sealed up everything with silicone.Freind gave me some AO, but when I used it it blew out of every crack in my cabinet.I was runing no more air than when I had glass bead in it.