Default Re: Aluminum Valve Cover Question

Quote:
Originally Posted by ptim
Not exactly what I wanted to hear, I guess this is the best they will get. Kind of gives me a bad taste on my first polishing job. They will get Powder Coated. Any powder coating experts out there, that could give me some advice on how this will look.
There's a powder coating forum in here too...(and don't discount the plating thing, it could be cheaper than you think...check the plating forum - also there's a "services needed" forum).