Tuch the bar compound to the spinning buff only for a second or 2
the compound will only last on the wheel for one minute or so
Just dab the bar, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff,

Then switch compound and, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff, dab, buff,

Welcome to the wonderful world of polishing