Re: Clearcoat is cracking.....
So your saying to use the flow out to determine the length of time, or the actual part temp?
I coated my first batch of powder and was confused on this.
The powder started to flow out way before the part ever reached the specified cure temp.
Specified cure temp 390, started to flow at about 225, where do you start your time at? At what point will clear start to yellow or cloud up?
|