Re: Powder Powder Everywhere, Newbie
Here are a couple of pics of the booth. Also there seem to be quite a bit of powder that falls to the bottom of the booth. Is this a normal amount for the two small parts I did? or am I doing something wrong? And one other thing, what would be the best way to go about cleaning up the booth/powder? Can I use a shop vac to clean up the excess powder? Any help or suggestions would be greatly appreciated. Thank you.
|