Quote:
|
Originally Posted by UrineMachine
I am planning on buying Xtreme Chrome and Candy Gold as a top color. Can anyone recommend finishing procedures? My friend who did the coating for my parts has the Hotcoat setup. Will it provide enough power to do this type of finish?
|
candy gold over chrome plating looks nice . over polishing also but over extreme or near chrome it looks more like a butterscotch color not very nice i my opinion