Default Re: Xtreme Chrome + Candy Gold?

Quote:
Originally Posted by UrineMachine
What is the best procedure for applying it? I will be doing it over xtreme chrome using an Eastwood kit. Any recommendations?
Fully cure the xtreme. Some will let the part cool to room temp before the Candy Gold and some will shoot it at about 150 degrees, your choice (maybe a few test pieces are in order). If you can turn down the voltage for 2nd coats, do it. Make sure you have a good ground.