Thread: hard anodizing
View Single Post
  #2 (permalink)  
Old 02-28-2007, 10:18 PM
acidrain acidrain is offline
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 881
acidrain is on a distinguished road
Default Re: hard anodizing

Never tried it but, the biggest problem will be getting acid temp down to around 32f, and holding it there while you hit it with 18+ amps CD.
At 18 amps CD, it will take 2 hrs to build 3mils with a peak voltage of 45v.
Is your PS able to handle that?
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote