Shooting a single colour piece can be straight forward, but when it has more detail, like if the customer wants to leave the lettering on an intake uncoated you seem to have to invest a lot more time carefully taping off the area. I was just wondering if it might be easier, and work just as well, to spray the whole piece and then wipe off what you don't want with a damp cloth before baking it. What do you think?