Originally Posted by Banditperformance
I kind of take an average. If the lower temps are alot colder, then wait till they get closer. MOst powders ahve areally good overbake, up t a Hr for some powders. SO, the areas that reach cure temp first are not going to overcure by the time the other areas cure. Most powders start flowing at 360F as well, curing at 380. Lower cure temps, just mean longer cure times.
That seems high to me.