I painted cars for many years. I used a metal/Paint prep before I would spray paint. It removes any finger prints or any other surface contaminants that may have landed on the surface. I have also started using it for powder coating. You can get it at any Auto Paint store and some car parts stores. Some of it you just put it on and your done, some others you have to follow up with another rag to dry. Don't get that one. I've read here and I've done it myself, use carb cleaner in the spray can or brake cleaner. No petroleum.