Send a message via AIM to lfsracing
Default Re: Powder coating something zine plated?

Yeah that's what I just did. We just used 100 grit sandpaper and it came off really easy I figured it would as it coudln't of been thick to begin with. I will get them cleaned up shortly and I have to PC some of my stuff so figured I can do them for him.
Lorenzo