You don't mention the surface prep you used, or what kind of nickel plating system you have. It doesn't sound like one of ours, based on the size of the nickel anodes. If it is one of ours, please post a problem report in our PRS system.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote