Default Re: Is PC Conductive?

Quote:
Originally Posted by vertek
I think it has a certain conductivity, but all things do,
when it cure's i think it becomes an insulator because people complain that theyr hooks that they use for hanging stuff have lost conductivity, and they have to blast em clean.
Thanks - so it could very well isolate a ground plane from a car if the means of completing ground is based on contact with the now powder coated surface.

Proves my theory, but running a dedicated ground didn't fix my problem. Oh well, was worth a shot!