Re: Spray Booth questions - many
also depending on how big the squirrel cage is you may be moving more air than you want. I don't get to worried about reclaiming and using the powder again. You should be worried about a top quality finish and if your customer appreciates the professional finish you put on the item then he will be more than happy to pay you for your efforts and your name will be passed on. If you reuse the powder to save a buck and the finish has flaws your customer will not be happy. Don't let a buck stand in your way with perfection. Every job you do is an advertisment and your NAME is on it !!!!!!!!!!!!!!!
|