Question regarding the clear.

Shot my son's chrome air cleaner with Psycho Lime Green, and there were "bumps" in various places, almost like there was some dirt trapped on the cleaner. I scrubbed the **** out of it and rubbed it down with de-natured alcohol before I shot it.

Next step was to apply Caswell's 120% super high gloss.............again, looks like there was dirt on the cover. Some parts of the clear coated beautifully, in many other places, this appearance of dirt........

Maybe I shot the green / clear too thick?