Default Re: Sealing grey BL dyes?

I have only used it twice, and each time the surface was dull, and keeping the sealer boiling long enough for a couple racks is troubling, plus the evaporation of the sealer. I use an LT sealer from Ron Newman that I have great results with. I do still have about a half of bag left of Caswell's high temp sealer. I quess I will try it again, any pointer on getting good results?