View Single Post
  #16 (permalink)  
Old 03-11-2007, 01:57 AM
callmej75 callmej75 is offline
Amateur Metal Finisher
 
Join Date: Feb 2006
Location: Roanoke, VA
Posts: 185
callmej75 is on a distinguished road
Send a message via Yahoo to callmej75
Default Re: Media Blasting Solution 5 Star!!

Quote:
Originally Posted by cdaeme
The tanks are only pressurized to 10-25 psi. The PA stands for "pressure assisted". These are much safer to operate than conventional pot blasters. I have considered building 3 or 4 of these pvc setups and putting different media in each with switching valves to change between medias. Just dump whats in the cabinet and switch to the next media.

Jason
Ohhhh....so this actually helps blast more off at a lower PSI? Or about the same? Regardless its at a lower psi than now and burning up tips all of the time.
Reply With Quote