View Single Post
  #1 (permalink)  
Old 03-11-2007, 04:49 PM
LCC LCC is offline
Newbie
 
Join Date: Mar 2007
Posts: 6
LCC is on a distinguished road
Default What am I doing wrong?

I'm new to polishing and had a question or two. I'm starting out with a 1/2" piece of aliminum. I'm using a bench grinder 1hp @ 3500rpm with 6" buffing wheels. First step was wet sand with 400 in a crisscross pattern, then to 600 wet. After that it appeared In good shape to go to the wheels. Started with brown and got a pretty good finish but some pits and hairline scratches. I thought the scratches were from the brown so I continued onto a seperate wheel with red. Some scratches came out and the shine got a little better but I continued using the red awhile until the aluminum was almost to hot to hold with bear hands. It seemed to get worse after awhile with milky streaks in it. Did I heat it too much? and I still have some hairline scratches. I'm not sure which direction to go now.

Thanks for any help.
Reply With Quote