Re: can I remove 'hard coating' (type 3)?
With any stripper, you have to watch it, and help it along by scrubbing with a toothbrush or whatever.
The key is to leave it in only as long as it takes... too long and it will dull.
I always buff or beadblast afterwards anyway, so it's no big deal.