0.0625" Titanium Wire
Guys:
I bought some 1/8" Ti rod from a guy a few weeks ago. He emailed me today and said he has 6 pounds of 1/16" X 36" Ti-1 welding rod for sale for $140.00. I think that figures out to be 300 sticks and I think he wants to sell the whole lot at once.
It may go quick (he said first come, first served) , but if anyone is interested, PM me and I'll give you his email address.