i just completed my oven, works fine for PC 400* in about 15 min. has anyone worked past that temp? i want mine to get to 700*, for ceramic coating. it took another 15 min. for it to get to 500*, then we had to quit, tomorrow i will see how long it takes to get to 700*, hope it wont take an hour, that would be a bummer.

if i need to add more wattage, can i run a second contactor with split power in and a switch? if i dont need the second set of elements i can turn the switch off and just run off of one set.