The acetone may be the problem. I've had similar problems with diecast and it stopped when I switched to SP degreaser. I also follow that step with Lava soap (of course, I'm plating little things, don't know how that would work with something bigger). Water sheeting is a pretty good test to see if everything is completely rinsed.
|