Default Re: road to a new blast cabinet

I live a few miles away from the grizzly industrial warehouse. I went there yesterday to get an upgrade gun for the blaster and found that they sell a nice blaster gun recommended by many. While there i also found that grizzly has carbide tips for the gun. As a little mod i converted over to carbide and also made a better jet at 5/32ths instead of the factory 3/32ths jet. I highly recommend the conversion. If anybody needs one of these setup i can get them to you cheaper since there will be no cost for the rejet and I have cheap shipping compared to the grizzly. I also have a second fully built unit ready to go if anyone needs one.