Default Re: Copy Cad Help (Power Supply Problem ?)

Hi Seanc, my part is not that big, is it ? help me put my lack of confidence in my math to bed . Am I working this out right ? my part in question is 6"x5" and I am plating both sides so I multiply x2 , = 60" is this correct ?
If I am correct then I now do have a power supply problem as my bench top supply only puts out 3.12A max.
I tried the piece this evening at my max 3.12A and saw a little fizzing for the first time, it turned out with shiney nice plate on a few areas but still dark on others, so I think I am heading in the right direction, looks like I need a bigger power supply and some more anodes. Can I buy regular zinc anodes from another supplier, or do I have to use the Caswell ones ?