Default Re: Powder color sample packs?

Well buying 20 different colors and only being able to use 8 or 9, selling the rest for less than half of what i paid doesnt make a whole lot of sense to me..

The the 2 colors I was really surprised by was Teal and Green, the paint chip for teal looks about what the powder looks like but the picture is way wrong, the green paint chip seems to be the lightest of the greens with pictures(turf and tropical) but it is the darkest forest green I have ever seen, the turf green pic looks almost neon. I think some of the pics are wrong

A picture of the raw powder would be alot better than just the paint chips.


your right 4oz powders wouldn't work, 2oz would be better for samples and 8oz for regular selling sizes.


Caswell any chance this could become an option??

who's with me!!
Reply With Quote