My latest piece. Orange 3a with deep red in it. About 15cc red/ ½gallon orange. Matches the KTM very well.

Its done with 6 ASF for 2h. The CC powersource makes it all soo much easier and I also bought an aquarium-pump to swirl the water and make a more even temp and it works wonders. Huge difference in anodize thickness, much more even.
Here is a couple of pics.