I did re-cure it. But after I sanded it smooth, I cured it for 30 at 400. It took it quit awhile to get to that temp. The item, not the oven. It came out smooth, but didn't have the shine that another part I did at the same time did. More of a smokey chrome, but shinny. And picked a couple of, fish eyes? Need to get my act together!!! picture included.