I'd do Black first, full cure. Then tape, spray chrome. Bake till gloss over/flow out, 15 min or so. Remove tape and shoot clear. Then bake for remainder of chrome time.

I seem to have great results with half baking chrome, 10-15min, then shooting clear, and baking anopther 15. Cures the chrome and the clear. ANd the chrome stays more chrome looking. Doesn't oxidize as much.