Default copper over silver

I have a small metal trumpet tube that is brass with silver plating. The silver plating is about 50% worn off and has some pitting. What I want to do is plate over the piece with copper, without removing all the silver, and then final plate with silver.

Can copper go over silver?

Also, what is the difference between the silver in 4 oz bottle and the larger bottle that is cyanide free?