Would you allow a part to cool down in the oven if you are using a large oven (ex:96 cu ft int.) and then reheat the oven? Also on base color that you are shooting a second coat on (I have found that a semi-hot part takes a second coat better), do you let the part cool in the oven then or remove to a warm temp and then second coat.