Your 50KV Hobby Gun needs.......
A lower voltage setting! The regular 14KV gun works much better on tight spots. The 50KV guns lowest setting is over twice the voltage as the regular gun. Add a switch to the gun that allows it to adjust down to the same voltage as the cheaper gun. The new gun also makes it harded to get a Non-Orange peeling finish. I am having to finish the part off with the gun OFF in order to get less orange peel.
|