it can be done very easily. just make sure to clean the calipers very good. if they have any oil, brake fluid or rust on them it will bubble the powder. if u are doing them for ppl, i always run the idea from them to look at buying new ones from an auto parts store. they are fairly cheap and they are clean and ready to go after a wipedown. here is a set i played with the idea of lettering on them.