Quote:
Originally Posted by wrascal
I tried using the extreme chrome on a steel rim and when I coated the high gloss clear, it did not go flat, but melted into little blobs. I baked it at 400degrees for 20 minutes (checked the temp with an infared thermometer) Any ideas what I did wrong?

Russ
I ran into something similar to this a couple of weeks ago. It was on steel wheels and they has a build up of silicone on them and the brake cleaner will not remove silicone.

Jason