View Single Post
  #3 (permalink)  
Old 04-04-2007, 12:27 AM
baz baz is offline
Experienced Metal Finisher
 
Join Date: Feb 2006
Posts: 323
baz has a spectacular aura aboutbaz has a spectacular aura about
Default Re: A few questions from those that know.

i agree with harleydad but when i have different substrates i set my cure cycle on the heavier parts , most powders can easily support overcure as long as you don t over temp. but if the difference in substrate is extreme then i start my bigger parts then after about 15 minutes i add the smaller ones