View Single Post
  #3 (permalink)  
Old 04-04-2007, 08:21 AM
Ready2Dye Ready2Dye is offline
Newbie
 
Join Date: Mar 2007
Posts: 22
Ready2Dye is on a distinguished road
Default Re: I got SCREWED!!!!!

Quote:
Originally Posted by Ready2Dye
..some ideas (other than a racks)...

..some of you using ti c-clams...

A racks?

c-clams?? i meant c-clamps

wtf? It was 5:30PM- I wanted to go home. (So... what does proofread mean?)

Anyways...

Thanx destroyer for the info. I appreciate it.


Here is an example of why I want holes ano'd. Notice the spot that didn't ano where the wire made contact and of course the threading was not ano'd cuz of the screw- but it was on the other hole (not in this pic) and it looks like poop. FYI, with this part I am just gonna tap a 10-32 hole on top to attach the wire, it will be hidden when assembled. AAAANNY other suggestions are welcomed.

PS.. Can someone maybe PM me instructions on inserting an image (not an attachment) from my local computer (not http://). I see others have pictures right in their posts (no need to click on them), are they uploaded or are they hosted?

Thanx.
_
_
Attached Thumbnails
i-got-screwed-phpozfagram.jpg  
__________________
REDRIVER: You're still using the cool aid as a dye supplement aren't you? Avoid this...

quadster: Kool-aid? Hummmmmmmm............ I havent even tryed Rit yet yet.....I could clean out a bunch of cabinet space....

mcaswell: Cool Aid? RIT? ...Will someone pour me a large JD to steady my nerves?
Reply With Quote