You can make inside or outside clamps from the 1/8in Ti, and fasten them to cross pieces like shown below. I have 1/16in Ti that I use for smaller stuff like eye covers.
To insert an image, use an image host like Photobucket (it's free), and upload your pics to thier server. They have a link that you just copy and paste to your post.