View Single Post
  #3 (permalink)  
Old 04-05-2007, 08:41 PM
alabama_lowlife alabama_lowlife is offline
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 88
alabama_lowlife will become famous soon enough
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

use black first then white. always use a different wheel for each compound. and if you've got those sanded to 3000 grit, you'll only be stepping backwards with black, just use white and see how it turns out. if it's not good enough, then back up to black.
Reply With Quote