Thread: Curing question
View Single Post
  #3 (permalink)  
Old 07-12-2003, 12:54 AM
adambond adambond is offline
Newbie
 
Join Date: Apr 2003
Posts: 12
adambond
Default

are you using an IR (infrared) oven. if so its probably shortwave and they typically only heat the part surface quikly while taking longer to heat the sunbstrate . but you are probably using a regular electric oven im guessing, which evenly heats very well. maybe its cheap powder. ive had powder that wouldnt even resist rubbing alcohol.
ADAM (just trying to get a higher rating) BOND