copy chrome help needed
I have a 4.5 copy chrome kit doing a mostley aluminum. The first few came out good but now having problems with rough plate on some areas. looks like the surface creaters of the moon to frost on a window in the winter Tried every thing,from higheer temp to lower amps and double etching and zinkateing. Most of the time I have a dark haze on when I pull I out of the bath, buffs off ok, . I am not flash copper plating first and was wondering if I did flash copper plate first would that relieve those problems. My steel and copper things are fine. Please help any one !!!!!!
|