Strike Copper or Acid Copper over Nickel?
View Single Post
#
2
(
permalink
)
07-13-2003, 12:14 AM
mcaswell
Caswell Inc Founder
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,367
Blog Entries:
1
Flash Copper plate the steel, then nickel plate.
If you have acid copper, not Flash Copper, you need to nickel plate first, then copper plate, then nickel again.