ATV parts with gold color
I am in the process of rebuilding my sons ATV and I have noticed the wheel hubs and axle had a gold tint to them. Well I bead blasted the axle (which was steel) because of rust. And the hubs were aluminum, I washed with an aluminum cleaner. The gold tint was removed from the hubs. I think this gold tint was a Zinc coating and I wish to reapply this to both the hubs and axle. My question is whether this was a zinc coating?