Default Re: Looking for a good cheap gun

Ya, EW gun not really good. Get Caswells Vari-voltage gun. You will love it, trust me. I just did a bunch of pieces for a guy last week. He uses EW's gun. He saw Caswells gun and how the Podwer attracted to the part. He was amazed.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"