Default Re: PLATING POT METAL...............

Shawn there is very little Pot Metal on a Honda. It is all aluminum and cast at that. So you will have to re chrome it. after the copper plate hit it with nickel plate then Chrome it. That is the original triple chrome plating we hear so much about. You may find that just polishing the Aluminum and then covering it with a clear coat will look almost as good.take care dray