Yeah, you'll need a 25 amp 20 volt CC power sourse, but other than that everything else is basics.
You could mask the areas not needing ano like where the tire goes, and use a smaller PS.
The tank just needs to completely hold the rims with enough space to keep the parts at least 3in. from the cathode. A square-ish bin would be perfect.
I'm wondering about the cathode... you may want to have cathodes on each side of the rim to avoid shadowing.