I would think it would take almost forever with greaseless, since it wears off the buffing wheel fairly quickly and will need to be re-applied continually.

Those wheels need some serious sanding. I would probably start with something like 50 or 60 grit. Then 80, 120, 220, 400, 600 and then black emery. You need to grind off enough metal to where you have reached the level of the bottom of the pits and scratches. It may not be worth the effort. Given the labor involved, new wheels may be a better bet. Polish them.