Default Re: Can greaseless do the job? Pleasehelp

Quote:
Originally Posted by mpierich
Hey JR, how do you fill the holes? Or is the PC thick enough to bridge and level 'em? Multiple coats? Just asking, never tried it myself.
If the holes "pits" aren't to deep the powder will cover them, and yes you may need multiple coats. With deeper holes / road rash use Arvin's Lab Metal. Some have used JB Weld with good success!